Replacement Of Steel Slag And Quarry In Concrete

Replacement Of Steel Slag And Quarry In Concrete

Percentage steel slag and quarry dust to be replaced is found out by conducting 7days and 28 days compressive strength on cubes of sie 150 mm x150mmx150mm with 20 40 60 80 and 100 replacement of coarse aggregate by steel slag and fine aggregate by quarry dust. To study the strength loss weight loss characteristics of concrete.